SUMMARY
Preface 3
1. Background of welding process 5
2. Experimental and analytical investigations of fracture in weldments of 6082 Al alloy 35
3. Mechanical approach and FEM analysis 53
4. Fracture toughness of weldments in Al-Mg-Si alloy 68
5. Friction steer welding (FSW) general point of view about the method 107
References 133